(Just waiting for the kiln to finish firing, it's taking longer than I imagined it would, maybe because of the larger size)

Date: 2007-07-20 05:26 pm (UTC)
From: [identity profile] copper-oxide.livejournal.com
This firing the pots were pre-bisqued.
Fuel kilns are definitely able to fire faster than electric, assuming the kiln design is efficient.
That being said 4-6 hrs. is firing too fast for me though. I like my glazes to develop slooooow.

Date: 2007-07-21 02:41 pm (UTC)
From: [identity profile] earcmacfithil.livejournal.com
I've noticed that some glazes do indeed require more time to express certain attributes. Rutile blues are one. Copper reds and purples also seem to develop better with longer firings (so long as I don't overfire and volatilize all the Cu). With others, like clear, temmoku, copper green and cobalt, it doesn't seem to matter--in fact, the ones I use are fireable down to cone 8. On the other hand, my propane bisques have been extremely uneven as far as heat distribution, especially the ones I do in the Veragama (I hook up my Venturi burner for this.). In this case, I might indeed need longer firings in the 6-8 hour range or longer to avoid pinholing.

April 2019

S M T W T F S
 123456
78910111213
14151617181920
21222324252627
282930    

Most Popular Tags

Style Credit

Expand Cut Tags

No cut tags
Page generated Jan. 22nd, 2026 04:37 am
Powered by Dreamwidth Studios